HUAYU ADDITIVE 75TiF/ 80TiF/ 75TiAl/ 80TiAl

Description
Dark gray tablet additive.

Availability
To adjust and compound the content of Ti in aluminum alloys and to replace Al-Ti alloy.

Instruction
When the temperature of melt reaches 730-760¡æ, skim the slag off, add demanded additive, wait for 10 minutes and stir completely. Recovery will be more than 90%, test the Ti inclusion after 40 minutes.

Application Rate

Added volume=
                                Needed volume in Al alloys                                 
                           75%(or 80%)¡Á90%(percentage)
Note: the recovery of 75TiAl or 80TiAl can reach 95%.

HUAYU ADDITIVE 75 TiF 80TiF 75TiAl 80TiAl
•Easy for operation to reduce labor intensity
•it can avoid the oxide and the salt inclusion can purify the melt
•No Na inclusion, won¡¯t disturb the strontium content alloys.

Packing
G/tablet        Tablets/alum.Foil roll           Kg/ alum. Foil roll           Kg/carton          Remarks
   200                         5                                   1.00                           20.00 
   500                         4                                   2.00                           20.00 
   667                         3                                   2.00                           20.00            75TiAl
 
Storage
Store in dry warehouse. Avoid absorbing water.

Valid Date:   6 months.

Material Safety Data:

Appearance:      dark gray tablet
Density:          2.8-3.0 g/cm3
Color code label:   red

[Print] [Close]
 